Time:2024-04-18 Views:1 source:HF welding and cutting machine
1. In general; When the roller is loaded into the frame; In general, it will not be arbitrarily removed; However, the service life of the roller should be extended; The scientific method is to release the oil or water in the roller; Then through the anti-rust oil; When in use, the oil is released again; Cleaning and oil removal; Then use it in the normal way.
2. Warm or cool the roller before use; To adjust the roller to slow rotation; This is conducive to the roller heating or cooling will not be caused by its own weight cooling and heating uneven deformation; It is a kind of way to extend the service life of the roller.
3. When the roller is removed from the frame; The water inside should be removed; Then the roller surface on the anti-rust oil or butter and then with PVC protection packaging and then with soft packaging for packaging; This is conducive to protect the surface of the super mirror roller and the acidic or alkaline gas in the air chemical reaction; The surface finish is reduced because of the clumps. In severe cases, the roller surface will be repaired; Cause damage.
4. When the roller is not in use; Be sure to lay the roller flat in the protective frame; Anti-roll surface contact with foreign matter and damage its surface quality; At the time of loading or storage; Be sure to handle lightly; Damage is strictly prohibited.
5. The roller produces static electricity due to friction with the material being pressed; Will absorb the powder layer in the air to the surface of the super mirror roller; When more foreign bodies are found on the roll surface within a certain period of use; To use soft cloth or sponge items with wax products; Gently wipe the roller surface from left to right (back and forth); It is beneficial to extend the high quality of the roller surface.
6. Machine production; When all kinds of materials enter the roll face; To the material surface is not calendered position (open to the end); Because the material will not roll; Therefore, mobile scratches caused by rapid hardening of materials sometimes occur; To produce scratches on high finish surfaces; As agreed; If it does not affect the quality, it can be extended; Affect the quality of production materials; It is necessary to send the roller processing plant surface polishing treatment; If such problems are noted in production; The abnormal problems caused by the roller can be reduced to a minimum for extended use.
Read recommendations:
1.2M Automatic disc high frequency welding machine
Double Head High Frequency Plastic Pvc Welding Machine
Complete control over products allows us to ensure our customers receive the best qualityprices and service. We take great pride in everything that we do in our factory.